Description:
|
O-rings are made to contain thousands of PSI pressure by creating a seal between two or more parts. O-ring measurements are defined by the inside diameter and the thickness.
There are many causes for O-Ring failure. The most common among power tools are:
Extrusion and Nibbling – The O-ring has ragged, tattered edges. These are commonly caused by pressure spikes which shear off tiny “bites” from the o-ring, or caused by clearance gaps.
Abrasion – One or both sides of the o-ring appear rough and slightly flattened. Commonly caused by a contact surface that is too rough, contains grit or is too smooth to allow lubrication.
Over Compression – The O-ring is flattened on both sides and may have a “ring” split along its length. Commonly caused by excessive pressure or heat.
Heat Hardening – The O-ring has a pitted or cracked surface, and is often flattened on both sides. Caused by temperature exceeding o-ring capacity.
Weather/Ozone Cracking – The O-ring is covered in small surface cracks. Caused by exposure to ozone, UV rays and air pollution. Excessive seal stretching (greater that 5%) causes similar cracking.
|
Product Information:
|
Manufacturer: DeWALT | | Category Number: 323711-11 | | Classification: Part | | Ships to: United States and Canada | | Weight: 0.01 lbs. | |
|